Product description:
1:This production adopt advanced double dot coating technique.It has a good performance after dry and water washing with low shrinkage.
2:It widely suits for the materials of silk,cotton,polyester cotton,polyester viscose,chemical fibers,woolen etc.
3:It is suitable for the front parts,collar,sleeve,waistband,placket,pocketing and reinforcement parts of jacket,wind coat,overcoat and suits.
Product | Weight (g/㎡) | Width(Inch) | Base Cloth Composition | Coating | Powder | Weaving specification | Base cloth specification | Fusing Condition | ||
Temperature(℃) | Time(s) | Pressure (kg/cm2) |
||||||||
H1203W | 28 | 60' | 100%Polyester | DOUBLE DOT | PA | 30D | Plain 1/1 | 120~140 | 12~15 | 1.5~2.5 |
H1205W | 46 | 60' | 100%Polyester | DOUBLE DOT | PA | 50D | Plain 1/1 | |||
H1207W | 56 | 60' | 100%Polyester | DOUBLE DOT | PA | 75D | Plain 1/1 | |||
H1210W | 74 | 60' | 100%Polyester | DOUBLE DOT | PA | 100D | Plain 1/1 | |||
H1203Q | 28 | 60' | 100%Polyester | DOUBLE DOT | PA | 30D | Plain 1/1 | |||
H1205Q | 46 | 60' | 100%Polyester | DOUBLE DOT | PA | 50D | Plain 1/1 | |||
H1207Q | 56 | 60' | 100%Polyester | DOUBLE DOT | PA | 75D | Plain 1/1 | |||
H1210Q | 74 | 60' | 100%Polyester | DOUBLE DOT | PA | 100D | Plain 1/1 | |||
H1503L | 30 | 60' | 100%Polyester | DOUBLE DOT | PA | 30D | Plain 1/1 | |||
H1505L | 46 | 60' | 100%Polyester | DOUBLE DOT | PA | 50D | Plain 1/1 | |||
H1507L | 56 | 60' | 100%Polyester | DOUBLE DOT | PA | 75D | Plain 1/1 | |||
H1510L | 74 | 60' | 100%Polyester | DOUBLE DOT | PA | 100D | Plain 1/1 | |||
H1512L | 85 | 60' | 100%Polyester | DOUBLE DOT | PA | 100D | Plain 1/1 | |||
H1515L | 95 | 60' | 100%Polyester | DOUBLE DOT | PA | 150D | Plain 1/1 | |||
H1517L | 105 | 60' | 100%Polyester | DOUBLE DOT | PA | 150D | Plain 1/1 | |||
H1519L | 115 | 60' | 100%Polyester | DOUBLE DOT | PA | 200D | Plain 1/1 | |||
H1521L | 125 | 60' | 100%Polyester | DOUBLE DOT | PA | 200D | Plain 1/1 | |||
H1522L | 130 | 60' | 100%Polyester | DOUBLE DOT | PA | 200D | Plain 1/1 | |||
Due to the wide variety of existing fabrics used by the clothing industry, we suggest that the test of the interlining, fabrics and the machine should be tested before using. |